BOPP thermal lamination film
Minimum Order: 0
Quality/Safety Certification: 0.00
glossy and matte
Surface layer: BOPP
glue layer: EVA adhesive
SPECIFICATION & PARAMETER
Surface layer: BOPP glue layer: EVA adhesive Thickness: GLOSSY: 25μm(12+13) 27μm(15+12) 30μm(18+12) MATTE: 27μm(15+12) 30μm(18+12) Width: 310~1880mm Length: 100~3000M Paper core: 25.4mm (1 inch),58mm(2.25inches),76mm(3 inches) BONDING: less than 2
Process Parameter:
Equipment for thermal film: dry and wet film laminator lamination temperature: 95~105°C Roller pressure: 10-20Mpa Speed: 8-20 m/minDirections for using BOPP thermal laminating film:
Normal process temperature is 90°C-105°C, roller pressure and temperature vary with different types of paper, ink and machines. When using the film for the first time or do other treatment, try a small volume before mass laminating. Make sure the ink is dry before laminating. It will delaminate when the paper contains too much moisture and powder. Make sure put the material in a low-temperature, dry place.