Cobalt Base alloy , spare parts
Minimum Order: 0
Quality/Safety Certification: 0.00
powder metallurgy and casting Based on the advanced OERLIKON coated electrode production line from Switzerland,
Stellite 1 | 48 | 2.20 | 29.00 | 2.00 | 14.00 | 3.00 | 0.50 | 3.00 | Bal | 1.00 | valve seat inserts, bearing, cutter edge, etc. | |||
Stellite 6 | 40 | 1.00 | 29.00 | 1.00 | 4.50 | 3.00 | 0.50 | 3.00 | Bal | 1.00 | engine valve, high temperature & pressure valves and turbine balde | |||
Stellite 12 | 44 | 1.30 | 29.00 | 1.00 | 9.00 | 3.00 | 0.50 | 3.00 | Bal | 1.00 | high temperature and pressure valves, sawteeth, screw flights, etc. | |||
Stellite 21 | 23 | 0.30 | 28.00 | 1.00 | 2.50 | 5.50 | 2.50 | Bal | 2.00 | turbine blades, valve seat, brass casting die | ||||
Stellite 25 | 0.15 | 20.00 | 1.00 | 14.00 | 3.00 | 0.50 | 10.00 | Bal | 1.50 | high temperature and corrosion resistance sealing ring, extrusion dies | ||||
Nistelle C | 0.10 | 17.00 | 5.00 | 6.00 | 17.00 | Bal | sealing ring for high temperature and corrosion resistance | |||||||
Ni-Mang | 0.60 | 2.70 | 0.20 | Bal | 3.70 | 13.50 | hammer crusher, fusion welding of manganese steel parts | |||||||
STE 308-16 | 0.08 | 19.50 | 0.90 | Bal | 0.50 | 10.00 | 0.80 | 0.50 | for welding 18% Cr-8% Ni stainless steel | |||||
STE 308L-16 | 0.03 | 19.50 | 0.90 | Bal | 0.50 | 10.00 | 0.80 | 0.50 | for welding extra-low carbon 18% Cr-8% Ni stainless steel | |||||
STE 309-16 | 0.15 | 23.50 | 0.90 | Bal | 0.50 | 13.00 | 0.80 | 0.50 | for welding 22% Cr-12%Ni stainless steel and welding stainless steel to mild steel or low alloy steel | |||||
STE 309L-16 | 0.02 | 23.50 | 0.90 | Bal | 0.50 | 13.00 | 0.80 | 0.50 | for underlying base metals, dissmilar metals | |||||
STE 309Mo-16 | 0.12 | 23.50 | 0.90 | Bal | 2.50 | 13.00 | 0.80 | for welding 22% Cr-12% Ni-Mo stainless steel | ||||||
STE 309MoL-16 | 0.03 | 23.50 | 0.90 | Bal | 2.50 | 13.00 | 0.80 | for welding extra-low carbon 22% Cr-12% Ni-Mo stainless steel | ||||||
STE 310-16 | 0.20 | 26.50 | 0.75 | Bal | 0.50 | 21.50 | 1.50 | 0.50 | for welding 25% Cr-20% Ni stainless steel | |||||
STE 310Mo-16 | 0.08 | 26.50 | 0.75 | Bal | 2.50 | 21.00 | 1.20 | 0.50 | excellent sulfuric-acid corrosion-resistance, crack-resistance, etc | |||||
STE 316-16 | 0.05 | 18.50 | 0.90 | Bal | 2.50 | 12.50 | 0.80 | 0.50 | for welding 18% Cr-12% Ni2% Mo stanless steel |
Based on the advanced OERLIKON coated electrode production line from Switzerland, Shanghai Stellite is able to supply various kinds of coated electrodes including Co-base electrode, high-temperature-risistant electrode,high-Cr cast iron electrode and Tungsten Carbide alloy.