Polyester tire or fiberglass based on, APP or APAO,APO for surface and coating with Isolation materials
Production Introduction
APP Modified asphalt is waterproofing membrane, made from Polyester tire or glass fiber tire which impregnated and coated by Atactic polypropylene (APP) or Polyolefin polymers(APPO,APO) modified asphalt.
Areas of Application
Basement, underground garage, potable water tank, swimming pool, storage, subway, tunnel, nuclear power station, port, waterproofing in high temperature and high humidity region, ect.
Features
Excellent heat resistance, good low temperature performance, especially for high temperature and high humidity areas
Application
Surface treated brush Prime coating Split seam treatment Hot-melt adhesive Joint
Note
APP Modified asphalt must stand, no exceed two layer.
Avoid rain, sun, moisture, fire, and keep ventilation..
Technical Parameter
Performance | PY(Polyester tire) | G(glass fiber tire) | ||||
Type | I | II | I | II | ||
Fusible Content, g/m2 | 2mm | - | ≥1300 | |||
3mm | ≥2100 | |||||
4mm | ≥2900 | |||||
Impermeability | Pressure ,MPa | ≥0.3 | ≥0.2 | ≥0.3 | ||
Keep time,min | ≥30 | |||||
Heat resistance,°C | 110 | 130 | 110 | 130 | ||
No sliding, flowing, dripping. | ||||||
Maximum tensile ,N/50mm | Vertical | ≥450 | ≥800 | ≥350 | ≥500 | |
Horizontal | ≥250 | ≥300 | ||||
Breaking Elongation ,% | Vertical | ≥25 | ≥40 | — | ||
Horizontal | ||||||
Low temperature flexibility ,°C | -5 | -15 | -5 | -15 | ||
No crack | ||||||