Properties Test Method Condition Unit Strengthened PA Toughened PA Strengthened & Toughened PA Flame Retarded PA
N1G30 N1G45 N2G30 N2G45 N1R10 N1R20 N2R10 N2R20 N1RG15 N1RG30 N2RG15 N2RG30 N2FG00 N2FG30
Tensile Strength ASTM D-638 5mm/min MPa 180 230 190 240 70 60 80 70 75 120 80 130 55 144
Elongation at Break ASTM D-638 5mm/min % 3 1.5 2.5 1.5 50 80 40 75 5 4 4 3 5 2
Flexural Strength ASTM D-790 2.8mm/min MPa 250 310 260 330 80 70 90 80 100 155 110 170 110 213
Flexural Modulus ASTM D-790 2.8mm/min MPa
Izod Notched Impact Strength ASTM D-256 3.2mm,23ºC KJ/m2 24 28 10 15 60 90 50 85 20 30 10 15 4.5 14
Rockwell Hardness ASTM D-785 23ºC R-scale
Melt Flow Index ASTM D-1238 230ºC/10Kg g/10min
230ºC/21.6Kg
Mold Shrinkage ASTM D-955 %
Heat Distortion Temperature ASTM D-648 6.4mm
0.64/1.82MPa ºC 205 214 255 255 110 100 115 105 185 200 210 220 185 245
Vicat Softening Temperature ASTM D-1525 5Kg,50ºC/m ºC
Specific Gravity ASTM D-792 1.37 1.53 1.37 1.53 1.10 1.08 1.10 1.08 1.19 1.33 1.20 1.35 1.30 1.51
Water Absorption ASTM D-570 Immersion in water,24hr % 1.0 0.7 0.8 0.6 1.5 2.5 1.5 2.5 1.5 1.0 1.5 1.0 1.0 0.8
Flammability Property ASTM UL94 HB HB HB HB V-0 V-0
Features
strengthened Toughened Strengthened & Toughened Flame Retarded
GF30
PA6 GF45
PA6 GF30
PA66 GF45
PA66 PA6 PA6 PA66 PA66 GF15
PA6 GF30
PA6 GF15
PA66 GF30

PA66 PA66 GF30
PA66

Ads by Google



About Us | Contact Us | Help | Terms & Conditions
Hot Products: A | B | C | D | E | F | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z | 0-9
Copyright Notice @ 2008-2022 B2BAGE Limited and/or its subsidiaries and licensors. All rights reserved.