Periodic pulse welding, the thinnest can welding 0.05mm and single-sides welding double-sides formation for 8mm.
Main technical parameter
Items | Unit | Value | Remarks |
Input voltage |
| (three phase)380V 50HZ |
|
Rated welding current | A | 200 |
|
Rated duty cycle | % | 60 |
|
Pulse peak current | A | 1-200 |
|
Pulse base current | A | 1-200 |
|
Pulse frequency | HZ | 1-30 |
|
Pulse duty ratio | % | 10-90 |
|
Current rise/fall time | S | 0.5-5 |
|
Plasma gas flow | L/min | 0.1-1 |
|
Projection gas flow | L/min | 1-10 |
|
Power form |
| IGBT inverter-type |
|
l Periodic pulse welding, the thinnest can welding 0.05mm and single-sides welding double-sides formation for 8mm.
l Adding 3-5% hydrogen into the protecting gas to reduce welding oxidation.
l High speed welding, three times than argon arc welding.
l Fine seam formation, little deformation and as well as laser welding.
l Can weld steel, stainless steel and other alloy steel, such as Cu, Ni, Ti, Mo, W, Pt , Rh alloy or the special metal.