Welcome to B2BAGE
Cation Exchange Membrane
Cation Exchange Membrane

Minimum Order: 0
Quality/Safety Certification: 0.00


Mainly for hydrogen-oxygen electrodialysis, desalination, water electrolysis.

Cation Exchange Membrane

Color Light: Yellow

Standard Size: Metric 0.8m x 1.6m

Standard thickness(mm): 0.25-0.28

Electrical Resistance (Ohm/cm2 ) less than 4.0

Permselectivity (%) :96.2

Total Exchange Capacity (mol/kg) more than 1.4

Mullen Burst Test strength(Mpa) more than 0.9

Thermal Stability (°C) less than 50

Membrane potential(Mv) 14.9(14°CLiquid temperature)

Moisture Content(%) 40-70

transference number of ions less than 0.95

Storage: 

1, wet condition preservation. Homogeneous ion exchange membrane according to the 

different brand, shrinkage in 710 % respectively, between dehydrate condition will slowly

 contraction.

2, preservation temperature: 5-40%.

3, handling and storage, prevent extrusion, folding for damages caused to the deformation.

 

How to use: 

1, Open the package, carefully examine labels and cabinet material, lest produce errors.

2, roller is removed, the entire processing (cutting film, stiletto) and assembling process, the

 membrane surface must keep sufficient moisture, otherwise, it will lead to film contraction, 

the influence is used (can use sprinkling water bottles evenly to membrane sprinkler).

3, assembly, coping clapboard electrodialysis equipment before and isolated nets 

(key is welding parts) to inspect, be sure to level off, smooth, no burr, otherwise will 

membrane punctured, thus causing losses.

4, assembly electrodialysis equipment, should be careful operation and will end with the 

roller on the one end (right side clapboard alignment, alignment, then) along the clapboard 

downward end provinces, such as membrane expanded without betweent (deviated from 

clapboard) is required to reopen the roller is good, adjust good position to relaunch and may

 not be directly raise, or with membrane fingers hook lives film hole Angle adjustment, such as 

extremely easily, cause loss will tear film.

5, enter electrodialysis solution (or water) shall undergo pretreatment, feed unusualness

 degrees < 1, pollution index (namely mud density index) FI10 < 3-5 (ED)

6, electrodialysis equipment during the discontinuation, should maintain machine has 

sufficient moisture, otherwise it will cause membrane shrink and damage, need not when, 

best will membrane removed, soak in water.

Ads by Google



About Us | Contact Us | Help | Terms & Conditions
Hot Products: A | B | C | D | E | F | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z | 0-9
Copyright Notice @ 2008-2022 B2BAGE Limited and/or its subsidiaries and licensors. All rights reserved.