... physical property ,there are two different kinds of setting methods for PET staple fiber.One method is ... set under stress,so it called stressed heat setting.The other is to set at relaxed ... state,so it called relaxed heat setting.For ordinary cotton type,wool type,three dimensional ... fiber ,it must add a stressed heat setting machine,heat setting roller through steam or heat conduction oil,make ...