1.water reducing, high early strength, and high permeability enhancement
2..slow down the speed of hardening cement .
this product is compounded by high-efficient water reducing admixture and various retarders. It not only keeps the high-efficient water reducing admixture’s early strength and high strength sex, but also plays the role of slowing down the speed of hardening cement.
This product meets GB8076-1997 quality standard.
Homogeneity index
Test items | index |
Appearance | Light brown powder |
Solid content % | >90 |
Chloride ion content % | <1 |
Fluidity of cement paste mm | >180 mm |
Fineness(0.315 mm screen residue) | <15 |
Main performance:
the dosage is 0.6%~1% of the cement content ,water reducing ratio is up to 14%~22%No effect on early strength.Quan condense time can be extended by2-4 hours. Extending or shorting is available for special requirements.Heat time can be delayed; peak heat should be reduced in case of crack.
Quan performance index
Test item | First-rate product | Qualified product | |
Water reducing ratio( %) | >12 | >10 | |
Breeding rate (%) | <100 | <100 | |
Air content (%) | <4.5 | <4.5 | |
Difference of gel time | start | >+90 | ---- |
end | ----- |
| |
Compressive strenght ratio% | 1day | ----- | ----- |
3 days | .>125 | >120 | |
7 days | >125 | >115 | |
28 days | >120 | >110 | |
Shrinkage ratio % | <135 |
| |
Corrosion for rebar | no | no |