1.green waterproof coating
2.single component
3.good ageing resistance,high elastic
4.low demand of surface moisture content

 Product characteristics

 1. Non-pollution, non-toxic, it is a green product. 

 2. Could be direct use on dry or wet (no visible water) base surface of various materials.

 3. High elastic coating, excellent water-resistant and Chemical corrosion-resistant

 4. Excellent light reflection ability and ageing resistance. Good for building energy saving and environmental protection.

 5.Single component product, use after open it, easy and safety construction.

 6.It has better effect of waterproof anti-corrosion and durability than the traditional waterproof materials.

 7. has excellent combination property and cost effective advantages. 

 

Application scope

Can be widely use in Leak-proof, anti-seepage and anti-corrosion of building roof, basement, kitchen, lavatory, pool, bridge and tunnel as well as can be use to bone various floor, asbestos shingle and glazed brick.

 

Packaging and storage

— Plastic Barrels Sealed Packaging; 25kg/pail.

— Be storage in cool dry place, against sunshine and frozen. Since the day of production the expiry time is 12 months. It can still be used if it beyond the expiry time while it’s tested qualified.

 

Performance indexes

No.

experimental projects

technical indicators

1

Drying time (h)

Surface drying time

≤4

Actual drying time

≤8

2

Solids content (%)

≥65

3

Tensile strength(MPa)

≥1.5

4

Elongation (%)

≥300

5

Low temperature and flexible

−20°c, no rack

6

Imperviousness (0.3MPa, 0.5h)

impervious

 

Notices

1. Construction temperature should be above 5°C. Open-air project avoid rainy days or avoid construct on base surface with water.

2. Do not do second coating until the first coating is dry.  The construction of protective layer or decorative layer should be only after the first coating is dry.

 

 

 

Ads by Google



About Us | Contact Us | Help | Terms & Conditions
Hot Products: A | B | C | D | E | F | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z | 0-9
Copyright Notice @ 2008-2022 B2BAGE Limited and/or its subsidiaries and licensors. All rights reserved.